FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade
1. What is Pre-alloyed Powder
Pre-alloyed powders are harder, less compressible and hence require higher pressing loads to produce high density compacts. However, they are capable of producing high strength sintered materials. Pre-alloying is also used when the production of a homogeneous material from elemental powders requires very high temperatures and long sintering times. The best examples are the stainless steels, whose chromium and nickel contents have to be pre-alloyed to allow economic production by powder metallurgy.
2. The Parameters of FCNS03
Main Element | Fe, Cu, Ni, Sn | |
Theoretical Density | 7.98g/cm³ | |
Sintering Temperature | 830℃ | |
Bending Strength | 1150Mpa | |
Hardness | 104-108HRB |
3. FCNS03 Character
4. Instructions for Making Ceramic Cutting Blade.
B. Diamond Grit Size and Percentage:
C. Sintering Temperature: 840-860℃